PCB edge beveling machine operation manual: A. Unpacking and installation When unpacking, first check that the outer packaging is not damaged. If there is any damage, contact our factory. If there is no damage, open it carefully. Put the machine into a suitable position, and adjust the feet to a level. Check whether the machine …
Causes of corrosion of metal etching side
Why is there side corrosion in the metal etching process? The two most critical and at the same time the most important parameters in metal etching. The etching speed determines the length of the etching processing cycle. The faster the etching speed and the shorter the etching processing cycle, the higher the production efficiency, and …
Circuit board pth (plating through hole), npth (non-plated through hole), via (via hole) use introduction
We often see large and small holes on circuit boards. Holes can be roughly divided into PTH (Plating Through Hole) and NPTH (Non Plating Through Hole). “It’s because this kind of hole really penetrates from one side of the circuit board to the other. In fact, in addition to the through holes in the circuit …
Etching machine
Etching machines can be divided into chemical etching machines and electrolytic etching machines. In chemical etching, a chemical solution is used to achieve the purpose of etching through a chemical reaction. A chemical etching machine is a technology that removes materials by chemical reaction or physical impact. Automatic etching machine: The automatic chemical etching machine …
What kinds of tin spraying are available for the surface treatment of PCB circuit boards
PCB circuit board tin spraying, also called hot air leveling, is an important process in the production of PCB circuit boards. The surface treatment of PCB circuit boards can be divided into two types: lead and lead-free: Lead HAL The so-called lead-sprayed tin refers to the tin in a certain proportion, and the lead will …
Print Circuit board developing machine process
The developer of the water-soluble dry film is a 1-2% anhydrous sodium carbonate solution with a liquid temperature of 30-40°C. The development mechanism is that the active groups in the unexposed part of the photosensitive film react with the dilute alkali solution to generate soluble substances and dissolve. During development, the active group carboxyl-COOH interacts …
The difference between electroplating gold line and electroless gold plating line
The difference between electroless gold plating and electroplating gold (electroless gold plating is also called immersion gold; gold plating usually refers to electroplating gold). 1.The difference in principle FLASH GOLD (electroless gold plating) uses the method of chemical deposition! PLANTING GOLD uses the principle of electrolysis! 2.The difference in appearance Electroplating gold has electro-gold leads, …
Principle and process flow of PCB etching machine
With the development of the PCB industry, the impedance requirements of various wires have become higher and higher, which inevitably requires more stringent control of the width of the wires. In order to enable the engineering management personnel of Rongxin Company, especially the process engineering personnel responsible for the etching process, to have a certain …
Vacuum etching technology
Vacuum Etching Technology: An Improved Etching Technique for Ultra-Fine Structures. The etching process is a basic production step of PCB manufacturing. First, the resist is used to cover the wires and component pins that need to be retained on the copper-clad board, and the copper that is not covered by the resist and does not …
Dow Introduces New Automotive Adhesives
ecently, Dow Automotive Systems Division announced a cooperation agreement with Changan Automobile. Changan’s newly designed mini trucks and minibuses will use Dow’s BETAMATE 1620 structural adhesive. Dow’s innovative BETAMATE technology and on-site technical support and development of professional services not only meet the design needs of Changan, but also help it improve the strength and …